Galvanizers in  East Midlands

Frank Hand (Galvanizers) Limited

Frank Hand (Galvanizers) Limited

Address:
Colwick Industrial Estate,
Colwick,
Nottingham,
NG4 2AD

Telephone:0115 9870 508
Fax:0115 9400 793
Email: [email protected]
Website: http://www.frankhand.co.uk/

Bath size:
4.9 m x 1.5 m x 1.5 m

Double dip:
6.0 m x 0.25 m x 1.1 m or
3.5 m x 1.1 m x 2.2 m

Max lift:2 tonnes

Main classes of work:
General
Structural

Additional features and services:
Registered to BS EN ISO 9002
Grit blasting
Painting after galvanizing
T-Wash

Joseph Ash Galvanizing - Chesterfield

Joseph Ash Galvanizing - Chesterfield

Address:
Holmewood Industrial Estate,
Hardwick View Road
Chesterfield
Derbyshire
S42 5SA

Telephone:01246 854650
Fax:01246 850086
Email: [email protected]
Website: https://www.josephash.co.uk/locations/joseph-ash-chesterfield

Bath size:
16.2m x 1.6m x 2.3m

Double dip:
Sizes on application

Max lift:16 tonnes

Main classes of work:
General
Structural
Tubular
Castings

Additional features and services:
Registered to BS EN ISO 9001
Centrifuge for spin galvanizing
Grit blasting
Painting after galvanizing
Zinc spraying
Awarded ROSPA Gold Award 2016

Premier Galvanizing - Corby

Premier Galvanizing - Corby

Address:
Willowbrook Industrial Estate
Darwin Road
Corby
Northants
NN17 5XZ

Telephone:01536 409818
Fax:01536 409722
Email: [email protected]
Website: https://www.premiergalvanizing.co.uk/locations/premier-galvanizing-corby-2

Bath size:
7.5m x 1.3m x 3.0m

Double dip:
13.5m

Max lift:4.8 tonnes

Main classes of work:
Structural steel
Architectural steel
General fabrications

Additional features and services:
Collection and delivery service
Full technical support
On-site storage facilities
Packing and bundling
Shot blasting
Spin galvanizing
Powder coating

Worksop Galvanizing Limited

Worksop Galvanizing Limited

Address:
Claylands Avenue
Worksop
Nottinghamshire
S81 7BQ

Telephone:01909 486384
Email: [email protected]
Website: http://www.wedge-galv.co.uk/

Bath size:
20.5m x 1.32m x 2.4m

Double dip:
Sizes on application.
Max length approx. 29.0m depending on other dimensions.

Max lift:16 tonnes

Main classes of work:
General
Structural
Tubular
Castings
Wire work

Additional features and services:
Registered to BS EN ISO 9001:2015
Centrifuge for spin galvanizing
Grit blasting
Painting after galvanizing