Fire Resistance of Steel Sections Galvanized to EN ISO 1461

Galvanizers Association with the aid of Steel Construction Institute (SCI) has published a design guide which greatly simplifies the design of galvanized steel members in fire, avoiding any need for complex calculations.

The publication includes: 

Fire Resistance of Galvanized Steel