Corrosion Types

Corrosion Types
© Zsolt Palatinus
The types of corrosion for metals can vary in a number of ways dependant upon environmental conditions or design related issues. Protection to metals can be provided by a number of methods, one of which is by applying an additional coating that will afford corrosion protection. Consideration should also be taken into account with regards to the different types/mechanisms of corrosion. Some of the most common types are described below.

General Corrosion attack

This very common form of corrosion, attacks the entire surface of a metal structure. It is caused by chemical or electrochemical reactions. While general attack corrosion can cause a metal to deteriorate to point of failure, it is also a known and predictable issue. As a result, it is possible to plan for and manage general attack corrosion.

three types of localised corrosion

Localised corrosion

Pitting corrosion

Is a form of corrosion which results in holes or cavities within a metal.

Crevice corrosion

Corrosion that occurs in stagnant water often at joints, such as bolted connections.

Filiform corrosion

Occurs beneath coatings where humidity of circa 75%, and moisture and oxygen permeate beneath the coating.

Dissimilar metals in contact

Galvanic corrosion:

Galvanic corrosion normally occurs where two dissimilar metals are in direct electrical contact in the presence of an electrolyte which might commonly be condensation, rain water or sea water. Effectively a battery cell is created and an electrical current flows as a result of the corrosion of one of the two metals.

In essence, one metal’s molecules are drawn toward the other, leading to corrosion in only one of the two metals. It is the more electronegative metal in the electrochemical series which corrodes. Read more about galvanic corrosion. 